Eiendom | Eenheid | Toets metode | Standaard |
Lineêre digtheid | Teks | ASTM D1907 | 300±10% |
Treksterkte 1) breek 2) VERLOOP 0,3% 3) LASE0.5% 4) LASE1.0% | N | ASTM D 885 | Min.150 Min.24 Min.40 Min.80 |
Proporsie | g/cm³ | ASTM D1505 | 2,55±0,05 |
Young se modulus | Gpa | ASTM D885,D76 | Min.62.5 |
Verlenging by breek | % | ASTM D885 | 1,7-3,0 |
Absorpsie spoed | % | Min 150 | |
Absorpsie kapasiteit | % | Min 200 | |
Vog inhoud | % | Water blokkerende tipe | ≤1 |
Nie-water blokkerende tipe | ≤0,5 | ||
Opmerkings | Absorpsie slegs vir waterblokkerende tipe |
Postyd: 22-Sep-2022